Material Notes:
Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminating side.Availability: Latin America, North America and South AmericaKey Features:Excellent ink adhesion and bond strength in adhesive, PVdC adhesive, and extrusion laminationsNon-migratory slip system for consistent COFApplications:BakeryBiscuits/Cookie/Crackers Confectionery, Gum Confectionery, SugarCrisps and SnacksFresh Produce Uses:HFFS Flexible PackagingPouches – Flexible Packaging VFFS Flexible PackagingProcessing Method: Outer Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 4.30 g/m²/day
0.277 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
Thickness 30.5 microns
1.20 mil
Nominal; ExxonMobil Method
Coating Weight 27.4 g/m²
17.1 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.20
0.20
slip modified; ExxonMobil Method
Film Tensile Strength at Break, MD 124 MPa
18000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 241 MPa
35000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.0 %
4.0 %
at 275°F; ExxonMobil Method
Shrinkage, TD 4.5 %
4.5 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ExxonMobil Method
Gloss 88 %
88 %
45°, Untreated Surface; ExxonMobil Method
Descriptive Properties Value Comments
Wetting Tension 0.83 receding COS theta
Print Surface
Yield 25500 in2/lb