Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 60 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 75 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 18 LPX-2 OPP Film Product Description: Bicor LPX-2 is a one-side treated, one-side sealable OPP film designed for use in a lamination. It can be laminated to Metallyte, HBS-2, and itself to create lap sealable packag.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte® 25 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL-101 OPP Film Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 1311 Polyester Film Melinex® 1311 is a clear polyester film with antistatic properties on both surfaces for improved web handling and safety.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 581 Polyester Film A super clear, one side C-Sub pretreated film for adhesion of hydrophilic coatings.Approvals: UL Recognition - Product has been registered with Underwriters LaboratoriesInformation provided by DuPon.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OB13AF Polyester Film, 150 Gauge Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OL2 Polyester Film, 50 Gauge Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OL2 Polyester Film, 75 Gauge Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge Product Description: Mylar® RB42AF is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer and polyvinylidene chloride (PVdC) layer on the opposite side. .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RB43 Polyester Film, 100 Gauge Mylar® RB43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite side. Mylar® R.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Mylar® RL31 Polyester Film, 75 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ExxonMobil Method |
ExxonMobil Bicor® 110 ASB-X OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. ASB-X is good for heavy .. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 516 Polyester Film Melinex® 516 is a high clarity polyester film which is pretreated on both sides for slip to combine good handling properties with high clarity and brilliance.Typical Applications: Some typical uses.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB01 (formerly known as XM924) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and a polyvinylidene chlor.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |
|||
Film Tensile Strength at Break, TD | 241 MPa | 35000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 516R Polyester Film A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brillianceInformation provided by DuPont. |