ExxonMobil Bicor™ 18 LPX-2 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Bicor™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Bicor™ 18 LPX-2 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Bicor LPX-2 is a one-side treated, one-side sealable OPP film designed for use in a lamination. It can be laminated to Metallyte, HBS-2, and itself to create lap sealable packages.Availability: Latin America, North America and South AmericaKey Features:Excellent machinability as the outer web of laminations in HFFS and VFFS applicationsExcellent solventless adhesive lamination and wet-outExcellent ink adhesion and bond strengths in adhesive, PVdC adhesive, and extrusion laminationsLap seals to multiple coex sealantsNon-migratory slip system for consistent COFOptical print dot structure and minimization of pin-holingOutstanding graphic in both four and multicolor process print applicationsFeatures:In Lamination Lap SealableApplications:BakeryBiscuits/Cookie/Crackers Confectionery, GumConfectionery, SugarCrisps and SnacksUses:HFFS Flexible PackagingVFFS Flexible PackagingProcessing Method: Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Water Vapor Transmission 6.36 g/m²/day

@Temperature 38.0 °C
0.410 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 17.8 microns
0.700 mil
ExxonMobil Method
Coating Weight 15.7 g/m²
9.80 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.24
0.24
ExxonMobil Method
Film Tensile Strength at Break, MD 124 MPa
18000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 241 MPa
35000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.5 %

@Temperature 135 °C
4.5 %

@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 5.0 %

@Temperature 135 °C
5.0 %

@Temperature 275 °F
ExxonMobil Method
Optical Properties Metric English Comments
Haze 2.1 %
2.1 %
ExxonMobil Method
Gloss 85 %
85 %
45°; ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 216°F
Untreated
Wetting Tension 0.85 receding cos theta
Treated Surface
Yield 44000 in2/lb