ExxonMobil ESCOREZ™ 2184 (Europe) Petroleum Hydrocarbon Resin

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Adhesive
Manufacturer Exxon Chemical
Trade Name Escorez™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil ESCOREZ™ 2184 (Europe) Petroleum Hydrocarbon Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aromatic modified aliphatic hydrocarbon resin giving excellent compatibility with natural and most synthetic rubbers and with EVA copolymers. It is especially useful as a single tackifier for natural rubber based PSA formulations. Availability: Africa & Middle East and EuropeInformation provided by ExxonMobil Chemical.Appearance: Yellow Form(s): Pellets
Physical Properties Metric English Comments
Brookfield Viscosity 1000 cP

@Temperature 160 °C
1000 cP

@Temperature 320 °F
ETM E-31
Molecular Weight 1000 g/mol
1000 g/mol
Mn; ETM E-83
2300 g/mol
2300 g/mol
Mw; ETM E-83
Thermal Properties Metric English Comments
Softening Point 97.8 °C
208 °F
ETM based on ASTM D-6090-97; ETM E-24
Glass Transition Temp, Tg 45.0 °C
113 °F
ETM E-90
Optical Properties Metric English Comments
Yellow Index 82 %
82 %
Initial, Toluene solution with 50% resin in YI.; ETM E-13
Descriptive Properties Value Comments
Thermal Color Stability 150 YI
5hr, 347F (175C), ETM E-15