Polymer Property : Molecular Weight = 1000 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 1000 g/mol
1000 g/mol
Mn; ETM E-83
ExxonMobil ESCOREZ™ 2184 (Europe) Petroleum Hydrocarbon Resin
Aromatic modified aliphatic hydrocarbon resin giving excellent compatibility with natural and most synthetic rubbers and with EVA copolymers. It is especially useful as a single tackifier for natura..
Molecular Weight 1000 g/mol
1000 g/mol
C.O.I.M. DIEXTER® G215 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Molecular Weight 1000 g/mol
1000 g/mol
C.O.I.M. DIEXTER® G205 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Molecular Weight 1000 g/mol
1000 g/mol
BASF Pluracol® P1010 Specialty Polyol
Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used ..