Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil EXACT™ 0210 Ethylene-based Plastomer for Multilayer Film Applications

Category Polymer , Film , Thermoplastic , Elastomer, TPE
Manufacturer Exxon Chemical
Trade Name EXACT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXACT™ 0210 Ethylene-based Plastomer for Multilayer Film Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exact 0210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications requiring good flow/caulking and low SIT.Key Features:Low temperature heat seal performance including low seal initiation temperature and good caulking/flow.Superior toughness and tear strength.High clarity and low fogging tendency.High filler and oil acceptance.Low hexane extractablesAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaAdditive: Thermal StabilizerThis polymer complies with FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c) 3.2c, and may be used as articles or components of articles intended for use in contact with food, except for articles used for packing or holding food during cooking. Finished articles may contact food only under Conditions of Use C through H described in Table 2 of 21 CFR 176.170(c).Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ISO 1183
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
ISO 868
Thermal Properties Metric English Comments
Melting Point 97.2 °C
207 °F
Peak Melting Temperature; ISO 11357-3
Vicat Softening Point 75.0 °C
167 °F
ISO 306/A
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following: