Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 75.0 °C | 167 °F | B |
Plastcom SLOVALEN EQ 71 N PP, imp. strength FeaturesPE modified with EVA. The addition of EVA causes increased toughness. General application in all industry branches. Delivered in natural mode and in the full RAL colour scale.Packaging, tran.. |
|||
Vicat Softening Point | 75.0 - 108 °C | 167 - 226 °F | Average value: 95.5 °C Grade Count:98 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Vicat Softening Point | 75.0 °C @Load 1.00 kg, Thickness 4.00 mm |
167 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Vicat Softening Point | 75.0 - 129 °C | 167 - 264 °F | Average value: 114 °C Grade Count:11 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | |
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.Data was collected by ISO methods and o.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5056 500 Micron LDPE Powder Description: ICOFLO 510-5056 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Vicat Softening Point | <= 75.0 °C | <= 167 °F | |
JPJ Technologies LD 150 LDPE Virgin Applications: Used for heavy duty packaging, packaging bags, general film bag, etc.Information provided by JPJ Technologies |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Lushan M-20A Adhesive Resin for Multi-layer Oxygen Barrier Pipe Adhesive resin Lushan series for multi-layer oxygen barrier pipe is a modified polyolefin with functional groups. It’s designed to bond to a variety of barrier materials, such as nylon and ethy.. |
|||
Vicat Softening Point | >= 75.0 °C | >= 167 °F | ASTM D 1525 |
Karina E 835-10/155-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 75.0 °C | >= 167 °F | ASTM D 1525 |
Karina E 835-10/156-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 75.0 °C | >= 167 °F | ASTM D 1525 |
Karina E 835-10/91-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 75.0 °C | >= 167 °F | ASTM D 1525 |
Karina E 835-18/115-C-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 75.0 °C @Load 5.00 kg |
167 °F @Load 11.0 lb |
|
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM SILTEM-STM1500 PEI (Europe-Africa-Middle East) SILTEM STM1500 is a flexible siloxane-polyetherimide copolymer for cable and wire coatings. RoHS compliant. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Teknor Apex Sinvicomp SFR 5800C2 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Foamable Uses: Profiles; Foam Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | 50N-50°C per hour; ISO 306 |
Total PPC 7650 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7650 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a medium fluidity offering a combination of ease of processing and excellent impact propert.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | 50N-50°C per hour; ISO 306 |
Total PPC 9642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9642 is nucleated heterophasic copolymer. PPC 9642 is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and has been f.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | B (50N); ISO 306 |
Borealis Xmod™ PC75 High Crystalline Polypropylene Copolymer Xmod PC75 is a HCPP intended for injection molding of automotive interior parts. Xmod PC75 is a very easy-flowing material combined with a good balance between impact strength and stiffness. The m.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des.. |
|||
Vicat Softening Point | 75.0 °C @Load 5.00 kg |
167 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled PP copolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 75.0 - 77.0 °C @Load 5.00 kg |
167 - 171 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds ART 20 Rigid PVC, Atoxic for General Purpose Transparent bottles medium/high antishock |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Lushan M-8D Adhesive Resin for Coextruded Multi-layer Barrier Packaging Film Adhesive resin Lushan series for multi-layer barrier food packaging film has durable bonding properties when adheres to Polarity materials, such as PE, PP and PA, EVOH, etc. Adhesive resin Lushan se.. |