ExxonMobil Escorene® FL 00111 Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® FL 00111 Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FL 00111 is a copolymer of ethylene and vinyl acetate.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ASTM D2839/D1505
Vinyl Acetate Content 7.5 %
7.5 %
ExxonMobil Method
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Processing Properties Metric English Comments
Processing Temperature 190 - 200 °C
374 - 392 °F
blown film extrusion temp