Polymer Property : Processing Temperature = 392 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 190 - 200 °C
374 - 392 °F
Extrusion cylinder temperature, C1
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Processing Temperature 170 - 200 °C
338 - 392 °F
IRPC Polimaxx Polene G2865 High Density Polyethylene
CHARACTERISTICS: HIGH STIFFNESS, GOOD IMPACT STRENGTH, GOOD PROCESSABILITYAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DIARY PRODUCT BOTTLES, FRUIT JUICE BOTTLES, ONE-..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet
Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
KYDEX® V Acrylic/PC Thermoplastic Sheet
Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ..
Processing Temperature 150 - 200 °C
302 - 392 °F
Profiles
Lucobit Lucobatch® 1850 T100 Polyolefin TPO Granules
Lucobatch® 1850 T100 is a highly stabilized polyolefin based TPO granules. Lucobatch® 1850 T100 is employed as a master batch. Blended with suitable polyolefins, tunnel membranes are built of ..
Processing Temperature 150 - 200 °C
302 - 392 °F
Profiles
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Processing Temperature 190 - 200 °C
374 - 392 °F
Extrusion cylinder temperature, C1
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Processing Temperature 160 - 200 °C
320 - 392 °F
Profiles and hoses
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate
Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h..
Processing Temperature 160 - 200 °C
320 - 392 °F
Blow molding
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate
Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h..
Processing Temperature 180 - 200 °C
356 - 392 °F
Taiwan Sheen Soon Sheenthane® A8550 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 185 - 200 °C
365 - 392 °F
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 120 - 200 °C
248 - 392 °F
Fainplast Compounds Hax™ HFX 505 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com..
Processing Temperature 180 - 200 °C
356 - 392 °F
Resin temp
Asahi Kasei Tenac®-C EX351 Acetal Copolymer, Extrusion Grade  (discontinued **)
High-viscosity grade amenable to extrusion.Applications: Extruded rods and sheets.This product is not a part of the standard product line dated 2003.
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may..
Processing Temperature 150 - 200 °C
302 - 392 °F
Profiles
Lucobit Lucolit® 1310 Polyolefin TPO Granules, Grey
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Processing Temperature 150 - 200 °C
302 - 392 °F
Profiles
Lucobit Lucolit® 1320 Polyolefin TPO Granules, Beige
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..