Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® UL 8705 Adhesive Application Resin

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Exxon Chemical
Trade Name Escorene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® UL 8705 Adhesive Application Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has good compatibility with both hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, glue sticks, sealants and wax blends.Availability: Asia Pacific, Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsGlue SticksIndustrial SealantsLow Viscosity Adhesives Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ExxonMobil Method
Viscosity 9300 cP

@Temperature 190 °C
9300 cP

@Temperature 374 °F
ASTM D3236
Vinyl Acetate Content 27.6 %
27.6 %
ExxonMobil Method
Melt Flow 800 g/10 min

@Load 2.16 kg,
Temperature 190 °C
800 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
15s; ASTM D2240
Hardness, Shore D 18
18
15s; ASTM D2240
Tensile Strength at Break 1.93 MPa
280 psi
ASTM D638
Elongation at Break 360 %
360 %
ASTM D638
Flexural Modulus 0.0200 GPa
2.90 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 71.1 °C
160 °F
Peak Melting Temperature; ExxonMobil Method
Descriptive Properties Value Comments
Features Thermal Stabilizer