Material Notes:
Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low volatilities. Esterex™ Adipate Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many automotive and industrial lubricant applications. These esters are ideal in high-temperature conditions, such as reciprocating air compressors, where discharge valve cleanliness is required. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.928 g/cc

@Temperature 15.6 °C
0.0335 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 19
19
Index; ASTM D2270
Kinematic Viscosity 985 cSt

@Temperature -40.0 °C
985 cSt

@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 9.5 cSt
9.5 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 2.8 cSt
2.8 cSt
ASTM D445
Evaporation Loss 53 %

@Temperature 205 °C,
Time 23400 sec
53 %

@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -65.0 °C
-85.0 °F
ASTM D5950/D97
Flash Point 207 °C
405 °F
COC; ASTM D92
238 °C
460 °F
PMCC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4465
1.4465
ASTM D1218
Chemical Properties Metric English Comments
Acid Value <= 0.080
<= 0.080
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point <68°F
ASTM D611
Biodegradation 0.702
OECD 301F
Color <0.5
ASTM D1500
Composition Water
<50 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000756 (g/cc)/°C
ASTM D1250
Elastomer Compatibility -0.067
Fluoroelastomer Elongation Change, ASTM D471
-0.18
Fluoroelastomer Hardness Change, ASTM D471
-0.18
Nitrile Hardness Change, ASTM D471
-0.224
Polyacrylate Elongation Change, ASTM D471
-0.23
Polyacrylate Hardness Change, ASTM D471
0.281
Fluoroelastomer Volume Change, ASTM D471
0.413
Nitrile Volume Change, ASTM D471
-0.424
Fluoroelastomer Tensile Strength Change, ASTM D471
-0.449
Nitrile Elongation Change, ASTM D471
-0.55
Polyacrylate Tensile Strength Change, ASTM D471
-0.607
Nitrile Tensile Strength Change, ASTM D471
0.728
Polyacrylate Volume Change, ASTM D471
Fire point 460°F
COC, ASTM D92
Hydrolytic Stability, TAN Change 0.10 mg KOH/g
ASTM D2619
Kauri-Butanol Value 106.5
ASTM D1133
Noack Volatility 0.303
ASTM D5800/DIN 51581
RPVOT >1210 min
With AO, ASTM D2272
315 min
Neat, ASTM D2272