Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 123S (Nyeoil2) Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 168F (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 230A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 361F-BK (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 361FP (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362HF (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362HF-UV (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362HT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 390S-A(RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 715 (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 719A (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 719G (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 719G-CP (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 719L (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 719M (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 725A (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 732M (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 737B (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 737S (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 738 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 759M (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | Base Oil; ASTM D97 |
Nye Lubricants NYEOIL II Oil Information provided by Nye Lubricants. |
|||
Pour Point | -65.0 °C | -85.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® M30 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Pour Point | -65.0 °C | -85.0 °F | |
Dow Corning XIAMETER® PMCPPMX-200 350CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 350CS. 100% active, 350 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Pour Point | -65.0 °C | -85.0 °F | ASTM D5950/D97 |
ExxonMobil Exterex™ A32 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Pour Point | <= -65.0 °C | <= -85.0 °F | ASTM D5950/D97 |
ExxonMobil SpectraSyn Plus™ 3.6 Advanced Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices.. |
|||
Pour Point | -65.0 °C | -85.0 °F | |
Dow Corning XIAMETER® PMCPPMX-0210 Silicone Fluid 100CS Is chemically equivalent to DOW CORNING® 210H FLUID 100CS. This product is a heat stabilized polydimethlysiloxane, used for heat transfer.Information provided by Dow Corning |
|||
Pour Point | -65.0 °C | -85.0 °F | |
Dow Corning XIAMETER® PMCPPMX-200 100CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 100CS. 100% active, 100 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Pour Point | -65.0 °C | -85.0 °F | |
PolyOne Synplast™ DOA-N Di (2-ethylhexyl) Adipate Branched C8 adipate esterInformation provided by PolyOne |