ExxonMobil Exterex™ P61 Synthetic Fluid

Category Fluid , Lubricant
Manufacturer Exxon Chemical
Trade Name Exterex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exterex™ P61 Synthetic Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Esterex™ Phthalate Esters are API category Group V fluids. Esterex™ Phthalate Esters have excellent lower-temperature properties, good lubricating properties and low volatilities. Esterex™ Phthalate Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many automotive and industrial lubricant applications. These esters are ideal for use in air compressor applications, where low viscosity indices are acceptable and low-cost, clean operation is desirable.Appearance: Bright & ClearAvailability: Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.967 g/cc

@Temperature 15.6 °C
0.0349 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 62
62
Index; ASTM D2270
Kinematic Viscosity 11810 cSt

@Temperature -40.0 °C
11810 cSt

@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 38 cSt
38 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.4 cSt
5.4 cSt
ASTM D445
Evaporation Loss 15.3 %

@Temperature 205 °C,
Time 23400 sec
15.3 %

@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -42.2 °C
-44.0 °F
ASTM D5950/D97
Flash Point 209 °C
408 °F
PMCC; ASTM D92
224 °C
435 °F
COC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4829
1.4829
ASTM D1218
Chemical Properties Metric English Comments
Acid Value <= 0.070
<= 0.070
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point <68°F
ASTM D611
Biodegradation 0.714
OECD 301F
Color <0.5
ASTM D1500
Composition Water
<1000 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000724 (g/cc)/°C
ASTM D1250
Elastomer Compatibility 0
Fluoroelastomer Elongation Change, ASTM D471
-0.04
Fluoroelastomer Hardness Change, ASTM D471
0.046
Fluoroelastomer Volume Change, ASTM D471
-0.21
Nitrile Hardness Change, ASTM D471
-0.25
Polyacrylate Hardness Change, ASTM D471
-0.257
Nitrile Tensile Strength Change, ASTM D471
-0.289
Fluoroelastomer Tensile Strength Change, ASTM D471
-0.298
Nitrile Elongation Change, ASTM D471
0.39
Nitrile Volume Change, ASTM D471
-0.394
Polyacrylate Elongation Change, ASTM D471
-0.534
Polyacrylate Tensile Strength Change, ASTM D471
0.652
Polyacrylate Volume Change, ASTM D471
Fire point 514°F
COC, ASTM D92
Hydrolytic Stability, TAN Change 0.02 mg KOH/g
ASTM D2619
Kauri-Butanol Value 80
ASTM D1133
Noack Volatility 0.093
ASTM D5800/DIN 51581
RPVOT >2610 min
With AO, ASTM D2272