Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 209 °C | 408 °F | PMCC; ASTM D92 |
ExxonMobil Exterex™ P61 Synthetic Fluid Product Description: Esterex™ Phthalate Esters are API category Group V fluids. Esterex™ Phthalate Esters have excellent lower-temperature properties, good lubricating properties and low volatilit.. |
|||
Flash Point | >= 209 °C | >= 408 °F | |
ChevronTexaco Polystar® RB NLGI Grade 2 Texaco Polystar RB 2 delivers value through:Ability to meet bearing OEM requirements — Suitable for high rpm operations, operating temperatures ranging from -34°C to 204°C (-30°F to 400°F) and .. |