Material Notes:
Availability: North America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.663 g/cc

@Temperature 15.6 °C
0.0239 lb/in³

@Temperature 60.0 °F
ASTM D4052
Kinematic Viscosity 0.49 cSt
0.49 cSt
ASTM D445
Vapor Pressure 0.267 bar

@Temperature 20.0 °C
200 torr

@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties Metric English Comments
Boiling Point 60.0 °C
140 °F
Initial; ASTM 1078
Flash Point <= 0.000 °C
<= 32.0 °F
ASTM D56
Descriptive Properties Value Comments
Aniline Point 147°F
Method E, ASTM D611
Aromatic Content 0.002
ExxonMobil Method
Dry Point 145°F
ASTM D86