Vapor Pressure >= 0.267 bar
>= 200 torr
ASTM D279
Chesterton 296 Electro Contact Cleaner
Chesterton® 296 EU Electro Contact Cleaner (ECC) represents the latest advance in technology toward the search for more environmentally acceptable alternatives to CFC’s, HCFC’s, PFC’s, TCE & DCE..
Vapor Pressure 0.267 bar

@Temperature 20.0 °C
200 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Exxsol™ Isohexane Dearomatized Fluid
Availability: Africa & Middle East, Asia Pacific and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Vapor Pressure 0.267 bar

@Temperature 20.0 °C
200 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Exxsol™ Methylpentane Naphtha Dearomatized Fluid
Availability: North America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Vapor Pressure 0.267 bar
200 torr
3M Novec™ 7100DL Engineered Fluid
A higher purity version of 3M™ Novec™ 7100, 3M™ Novec™ 7100DL is tightly-controlled for ions, metals and non-volatile residue. It is used in precision cleaning and deposition applications when h..