Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glass, metals and paper.Applications: Golf ball covers; Injection molded articles; Foams; Impact modifiers.
Physical Properties Metric English Comments
Density 0.966 g/cc
0.0349 lb/in³
Exxon Method
Melt Flow 1.5 g/10 min
1.5 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength, Ultimate 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Flexural Modulus 0.175 GPa
25.4 ksi
ASTM D790
Tensile Impact Strength 520 kJ/m²
247 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Exxon Method
Vicat Softening Point 60.0 °C
140 °F
Rate B; ASTM D-1525