Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 520 kJ/m² | 247 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |