ExxonMobil Iotek® 7520 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Iotek® 7520 Zinc Ionomer Molding/Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK ionomers provide superb low temperature impact strength when blended with other polymers.Applications: Golf ball covers; Injection molded articles; Impact modifiers; Flexible tubings.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
Exxon Method
Melt Flow 2.0 g/10 min
2.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 30
30
ASTM D2240
Tensile Strength, Ultimate 12.0 MPa
1740 psi
ASTM D638
Elongation at Break 680 %
680 %
ASTM D638
Flexural Modulus 0.0400 GPa
5.80 ksi
ASTM D790
Tensile Impact Strength 780 kJ/m²
371 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 67.0 °C
153 °F
Exxon Method
Vicat Softening Point 40.0 °C
104 °F
Rate B; ASTM D-1525