Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-1060 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 19A Homopolymer HDPE Film Resin Film Properties.Data provided by the manufacturer. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9607D HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9607XD HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D4883 |
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D4883 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 69A HDPE Extrusion Resin
(discontinued **) Features: High tensile strength, better moisture barrier, better oil and solvent resistance, lower friction coefficient, lower brittleness temperature, better abrasion resistance, better temperature.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
Entec Hypel® PEHD.8/.962 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D 792 |
Total Finathene® 6450 HDPE film
(discontinued **) Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin.. |
|||
Density | 0.962 - 1.54 g/cc | 0.0348 - 0.0555 lb/in³ | Average value: 1.29 g/cc Grade Count:107 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Global B-6200 High Density Polyethylene Description-suitable for high quality blow molding, provides excellent surface glossiness in combination w/ outstanding environmental stress cracking resistanceApplications-cosmetics bottles, shampo.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Global J-2208 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Global J-2308 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene G2865 High Density Polyethylene CHARACTERISTICS: HIGH STIFFNESS, GOOD IMPACT STRENGTH, GOOD PROCESSABILITYAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DIARY PRODUCT BOTTLES, FRUIT JUICE BOTTLES, ONE-.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LB832001 High Density Polyethylene ApplicationsPETROTHENE LB 8320-00 resin is designed for sheet extrusion, vacuum forming and thermoforming. This resin exhibits very low sag, high stiffness.Regulatory StatusLB 8320-00 meets the req.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ISO 1183 |
Borealis Bormed™ HE9621-PH HDPE for Healthcare Applications Bormed HE9621-PH is a natural HD polyethylene with narrow molecular weight distribution, produced in low-pressure gas-phase process. This grade is designed for the injection molding of articles whe.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ISO 1183 |
Borealis CG9620 High Density Polyethylene CG9620 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Applications: CG9620 is recommended for coated film and co-extrusion.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ISO 1183 |
Borealis MG9621S Polyethylene MG9621S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9607 HDPE Cast Film Resin Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® C250 Polymer Modifier DuPont™ Fusabond® C250 is a modified ethylene vinyl acetate copolymer. Used as an adhesion promoter and coupling agent. |
|||
Density | 0.962 - 0.971 g/cc | 0.0348 - 0.0351 lb/in³ | ASTM D4052 |
ExxonMobil Jayflex™ DIDP Plasticizer (Asian Grade) Availability: Asia PacificCAS Number: 68515-49-1Information provided by ExxonMobil |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
Dow AMPLIFY™ GR 205 Maleic anhydride grafted (MAH) polymer AMPLIFY™ GR 205 Functional Polymer is designed as a blend component for unmodified polyethylene. In tie layers for flexible packaging, it promotes adhesion of polyethylene to barrier polymers such.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | |
Dow HDPE 10462N High Density Polyethylene DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | |
Abatron AboCoat 8006-3/8606-3 Clear Versatile Epoxy Clear epoxy protective and dielectric coatings. For spraying, brushing or rolling on metal, concrete, masonry, wood, fiberglass and most surfaces. Good adhesion, flexibility, hardness, water and c.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0339C10L1 Calcium Reinforced |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | |
BASF Isopropanolamine Formula: C3H9NOCAS: 78-96-6Description: Isopropanolamine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisopropanolamin, 1-Ami.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9608XD HDPE Film Grade This HDPE is tailored for applications that require:Very low gel levelsVery "clear" filmExcellent drawdownEnhanced stiffnessExcellent WVTR for a chill cast filmExcellent ProcessibilityTypical Cast F.. |