Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LDPE LD 258 Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 258 Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 258 is a LDPE extrusion coating grade, having superior organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers. The development of LD 258 reflects our in depth knowledge of the influence of extrusion coating process parameters as well as resin characteristics on the final odor and off-taste properties of coated materials.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrusion CoatingExtrusion CoatingExtrusion LaminationFood packagingHigh Speed, Thin Weight CoatingsIndustrial PackagingLiquid PackagingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 4.32 cm

@Temperature 315 °C
1.70 in

@Temperature 599 °F
656 ft/min, Constant output at 35 rpm; ExxonMobil Method
4.83 cm

@Temperature 315 °C
1.90 in

@Temperature 599 °F
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
Drawdown 7.17 m/s

@Temperature 295 °C
1410 ft/min

@Temperature 563 °F
Constant output at 35 rpm; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point <= 223 °C
<= 433 °F
Peak Melting Point; ExxonMobil method