ExxonMobil Label-Lyte™ 70LS447 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte™ 70LS447 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A two-side coated, shrink resistant, white, polypropylene film designed for use in hot melt cut-and stack labeling. It has an static resistant, matte finish, paper like print surface that is litho-printable, as well as compatible with water-based or solvent-based flexo and gravure inks and UV-cured inks. This film is deigned to be used as a monoweb and provides excellent converting performance, including printing, sheeting, guillotine cutting, and label transfer on magazine-fed labelers. The other side has a hot melt receptive coating.Availability: Latin America, North America and South AmericaKey Features: Excellent offset litho printing performanceExcellent static resistant properties for cut-and-stack labelingDurable and moisture resistantExcellent stiffness and burst performanceFeatures:Static Resistant CoatedStatic Resistant Matte CoatedApplications:Beverage, AlcoholicBeverage, Carbonated Beverage, Mineral Waters Dairy ProductsDry Foods and Beverage PowdersHousehold and DetergentsIndustrialUses: Cut & Stack (Hot Melt) LabelsProcessing Method: Conventional Offset Lithography Printing, Digital Offset (HP Indigo) Printing, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, Thermal Transfer Printing, UV Flexographic Printing, UV Screen Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
ExxonMobil Method
Coating Weight 51.5 g/m²
32.2 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 190 %
190 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 50 %
50 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, MD 89.6 MPa
13000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 165 MPa
24000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 5.5 %

@Temperature 135 °C
5.5 %

@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 5.5 %

@Temperature 135 °C
5.5 %

@Temperature 275 °F
ExxonMobil Method
Optical Properties Metric English Comments
Gloss 10 %
10 %
45°, Print Surface; ExxonMobil Method
Transmission, Visible 15 %
15 %
ExxonMobil Method
Descriptive Properties Value Comments
Opacity 90
Stiffness (Gurley) 29 mgf
MD
50 mgf
TD
Yield 13400 in2/lb