ExxonMobil Metallyte® 70 MET-HB OPP Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Metallyte®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Metallyte® 70 MET-HB OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A vacuum-metallized, high barrier OPP film with a proprietary sealant layer. This film offers excellent moisture and oxygen barriers, hot tack, seal integrity, and lap seal range when used with a coextruded outer web. MET-HB is designed specifically for adhesive and extrusion laminations. MET-HB resists crazing in extrusion laminations.Availability: Latin America, North America and South AmericaKey Features:Good oxygen barrierLow MST, broad seal range, strong sealsHigh adhesion of aluminum to filmResists crazing in extrusion laminationsExcellent hot tackFeatures: In Lamination Lap SealableLight BarrierMoisture BarrierOxygen BarrierApplications:Bakery Biscuits/Cookie/CrackersCrisps and Snacks Uses: HFFS Flexible PackagingPre-made Bags – Flexible PackagingVFFS Flexible PackagingProcessing Method: Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic PrintingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 0.190 g/m²/day
0.0122 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
Oxygen Transmission Rate 26.0 cc/m²/day
1.67 cc/100 in²/day
23°C, 0% RH; ExxonMobil Method
Thickness 17.8 microns
0.700 mil
ExxonMobil Method
Coating Weight 15.7 g/m²
9.80 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 152 MPa
22000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 234 MPa
34000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.5 %
4.5 %
at 275°F; ExxonMobil Method
Shrinkage, TD 2.5 %
2.5 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Optical Density 2.4
2.4
ExxonMobil Method
Transmission, Visible 0.40 %
0.40 %
ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 185°F
Crimp Seal Strength 400 g/in
205°F, 20psi, 3/4sec
Yield 44000 in2/lb