ExxonMobil Mobil 1 5W-30 Truck & SUV

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil 1 5W-30 Truck & SUV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil 1 Truck and SUV 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils. Mobil 1 Truck and SUV 5W-30 is engineered to help extend engine life in today`s hard-working trucks, SUVs, RVs and other gasoline powered vehicles. Mobil 1 technology has been selected as original equipment by car builders such as, Chevrolet Corvette, Cadillac, Mercedes Benz AMG, Porsche, Dodge Viper, and Dodge Ram SRT 10.
Physical Properties Metric English Comments
Density 0.800 g/cc

@Temperature 15.0 °C
0.0289 lb/in³

@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 169
169
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 64.8 cSt
64.8 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 11.3 cSt
11.3 cSt
ASTM D445
Ash 1.0 %
1.0 %
Sulfated Ash, wt%; ASTM D874
Thermal Properties Metric English Comments
Pour Point -54.0 °C
-65.2 °F
ASTM D97
Flash Point 230 °C
446 °F
ASTM D92