Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2020 LO-GC Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-GC is a glass clear pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging RB-FG Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® RB-FG is a clear, rigid PVC compound designed specifically for use as a color/ stability booster additive in Geon® packaging compounds where high regrind usage is necessary in extrusion blow.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Pyrotek A-1/S-1 Tadpoles A-1 glass fiber core with highly abrasion-resistant S-1 fabric jacket and mounting flange.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Pyrotek A-1/Z-5 Tadpoles A-1 rope core with jacket and mounting flange of densely woven glass cloth or wire reinforced glass cloth.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrot.. |
|||
Density | 0.801 - 1.36 g/cc | 0.0289 - 0.0491 lb/in³ | Average value: 1.22 g/cc Grade Count:123 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-1 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-17 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | M1433B; ASTM D1475-85 |
Lord Adhesives Aeroglaze® M1433 Elastomeric Polyurethane Rain Erosion Coating Aeroglaze® M1433 elastomeric coating functions exceptionally well in abrasive environments. Inherent flexibility, corrosion resistance, and energy absorptive properties make Aeroglaze M1433 elast.. |
|||
Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Solvay Chemicals CASO® FCC FLAKES Food Additive INS 509, Calcium Chloride CASO® FCC Flakes is a dihydrate calcium chloride food grade of mineral origin. According to the International Numbering System (INS) for food additives, CASO® FCC Flakes is characterized by th.. |
|||
Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Solvay Chemicals CASO® FEED POWDER Calcium Chloride Solvay is manufacturing and placing on the market dihydrate calcium chloride (CASO®FEED), feed material of mineral origin in conformity with European Directive 2002/32/EU and its amendments on u.. |
|||
Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Solvay Chemicals CASO® Powder CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4 / EINECS -.. |
|||
Density | <= 0.800 g/cc @Temperature 0.900 °C |
<= 0.0289 lb/in³ @Temperature 33.6 °F |
|
Solvay Chemicals CASO® TECHNICAL FLAKES LOW SULPHATES Calcium Chloride CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - .. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | <= 0.800 g/cc @Temperature 0.900 °C |
<= 0.0289 lb/in³ @Temperature 33.6 °F |
|
Solvay Chemicals CASO® TECHNICAL FLAKES Calcium Chloride CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - .. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Unifrax Fiberfrax® LDS Moldable Moldable Insulation Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b.. |
|||
Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Unifrax Fiberfrax® Pumpable-LDS Pumpable Insulation Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have te.. |
|||
Density | 0.801 - 0.961 g/cc | 0.0289 - 0.0347 lb/in³ | Dry |
Unifrax Fiberfrax® Vari-Form™ B Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Zircar Ceramics Z-500 Alumina-Silica Insulation Useful to temperatures of 1000°C (1832°F) Z-500 is uniformly rigidized and hard throughout its entire thickness, requiring no re-rigidizing after precision machining into complex shapes and confia.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1505 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Density | 0.801 - 0.961 g/cc | 0.0289 - 0.0347 lb/in³ | |
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | Foam |
Aptek DI-STRATE 1503 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: MicrowaveInformation provided by Aptek Labo.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | oven dried |
Pyrotek Pyrocast PT-60 Castable Refractory Pyrocast PT-60 is a ceramic fiber based insulating castable with very low thermal conductivity and excellent resistance to thermal shock.ApplicationsLaunder linings Distributor pan linings Ladle lin.. |