ExxonMobil Mobil Delvac 50 1650

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil Delvac 50 1650.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system.  They are specifically engineered for performance in intercooled, turbo-charged engines operating under severe on and off-highway conditions.  Mobil Delvac 1600 monogrades are used in a wide range of applications where a monograde lubricant is recommended.Naturally aspirated and turbo-charged diesel powered equipment; On-highway light and heavy-duty trucking; Off-highway industries including: construction, mining, quarrying, and agriculture
Physical Properties Metric English Comments
Density 0.896 g/cc

@Temperature 15.0 °C
0.0324 lb/in³

@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 110
110
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 202 cSt
202 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 19.5 cSt
19.5 cSt
ASTM D445
Ash 1.4 %
1.4 %
Sulfated Ash, wt%; ASTM D874
Thermal Properties Metric English Comments
Pour Point -18.0 °C
-0.400 °F
ASTM D97
Flash Point 290 °C
554 °F
ASTM D92
Chemical Properties Metric English Comments
Total Base Number 12
12
mg KOH/g; ASTM D2896