Thermal Properties Metric English Comments
Flash Point 290 °C
554 °F
Lubriplate 68 SYN High Temp 100% Ester-Based Multi-Purpose Synthetic Fluid
These 100% ester-based synthetic lubricants are recommended for applications that are exposed to high operating temperatures and must maintain a clean lubricated surface. Available in ISO viscosity ..
Flash Point 290 °C
554 °F
ASTM D92
ExxonMobil Mobil Delvac 50 1650
Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system.  They are specifically engineered f..
Flash Point >= 290 °C
>= 554 °F
ASTM D92, ISO 2592
Chesterton 610 MT Plus Synthetic Lubricating Fluid
Description: Chesterton® 610 MT Plus Synthetic Lubricating Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from 25°C (-15°F) to those o..
Flash Point 290 °C
554 °F
ASTM D92
ChevronTexaco RPM® SAE 140 Gear Oil
FeaturesChevron RPM Gear Oils are straight mineral gear oils. They are manufactured from specially treated high viscosity index paraffinic base stocks. They contain a metal deactivator to stop such ..
Flash Point 290 °C
554 °F
ASTM D92
ExxonMobil Mobil Delvac 50 1650
Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system.  They are specifically engineered f..