Material Notes:
Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
Tensile Strength, Yield 26.00 MPa
3771 psi
2 in/min; LAB032
Flexural Modulus 1.900 GPa
275.6 ksi
1% tangent, 0.05 in/min.; LAB033
Izod Impact, Notched 0.598 J/cm
1.12 ft-lb/in
LAB034
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
234 °F
LAB036