Material Notes:
White opaque OPP film with a proprietary cavitated core. Designed for cold seal applications and is used as a surface print, monoweb, or as the inside web of a lamination. Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 4.20 g/m²/day
0.270 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
Thickness 43.2 microns
1.70 mil
ExxonMobil Method
Coating Weight 28.2 g/m²
17.6 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 88.942 MPa
12900 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 162.03 MPa
23500 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %
5.0 %
at 275°F; ExxonMobil Method
Shrinkage, TD 5.0 %
5.0 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Gloss 65 %
65 %
45°, Print Surface; ExxonMobil Method
Transmission, Visible 24 %
24 %
ExxonMobil Method
Descriptive Properties Value Comments
Opacity 95%
Wetting Tension 0.8 receding COS theta
cold seal surface
0.9 receding COS theta
print surface
Yield 24200 in2/lb