Polymer Property : Thickness = 43.2 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 43.2 microns
1.70 mil
Nominal; ExxonMobil Method
ExxonMobil Bicor® 170 ASB-X OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. This film is suitable as..
Thickness 43.2 microns
1.70 mil
ExxonMobil Method
ExxonMobil Bicor™ 42MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent PP film, coated one side PVdC, one side acrylic, This film provides outstanding performance on all packaging machines.Availabi..
Thickness 43.2 microns
1.70 mil
ExxonMobil Method
ExxonMobil Oppalyte™ 42AH748 OPP Film
Product Description: A high barrier, high speed, super white opaque, modified higher density biaxially oriented polypropylene film, coated one side high barrier PVdC, one side very low temperature s..
Thickness 43.2 microns
1.70 mil
ExxonMobil Method
ExxonMobil Oppalyte™ 42MH647 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava..
Thickness 43.2 microns
1.70 mil
ExxonMobil Method
ExxonMobil Oppalyte™ 42MH648 OPP Film
Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated one side acrylic, one side very low temperature seal (VLTS) coati..
Thickness 43.2 microns
1.70 mil
ExxonMobil Method
ExxonMobil OPPalyte® 278 WOS-2 OPP Film
Product Description: One-side treated, on-side sealable, white opaque OPP film with a proprietary cavitated core. WOS-2 was developed to provide improvements over 278 WOS in terms of lower and more ..
Thickness 43.2 microns
1.70 mil
Total; ASTM D3752
3M 685 Riveters Tape
3M™ Riveters Tape 685 is a zone-coated polyester film tape with a tack-free center “window” for use in holding rivets in place both prior to and during riveting.Information provided by 3M
Thickness >= 43.2 microns
>= 1.70 mil
Side 1, Uncured Rubber Layer
Arlon 55579R043 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production materi..
Thickness 43.2 microns
1.70 mil
Tape Only
3M ATG 987 Tape
3M™ ATG Adhesive Transfer Tape 987 is a 1.7 mil, 400 acrylic, reverse wound, pressure sensitive adhesive on a densified kraft paper liner. Utility grade tape. For use with Scotch® ATG Adhesive App..
Thickness 43.2 microns
1.70 mil
estimated wet film thickness
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester
Thickness 43.2 microns
1.70 mil
Backing; ASTM D3752
3M 396 Super Bond Film
3M™ Super Bond Film Tape 396 is a polyester film tape for adhering to polyesters, polyethylenes and many other difficult-to-adhere-to surfaces.Information provided by 3M
Thickness 43.2 microns
1.70 mil
Adhesive
3M 7800 Aluminum Foil Label Material
3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78..
Thickness 43.2 microns
1.70 mil
Adhesive
3M 7801 Aluminum Foil Label Material
3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78..
Thickness 43.2 microns
1.70 mil
Faceside Adhesive
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
Thickness 43.2 microns
1.70 mil
Backside Adhesive
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
Thickness 43.2 microns
1.70 mil
Adhesive
3M 7940 Aluminum Foil Label Material
3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78..
Thickness 43.2 microns
1.70 mil
Adhesive
3M 7942 Aluminum Foil Label Material
3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78..
Thickness 43.2 microns
1.70 mil
ExxonMobil Method
ExxonMobil OPPalyte® 40 HM OPP Film
White opaque OPP film with a proprietary cavitated core. Designed for cold seal applications and is used as a surface print, monoweb, or as the inside web of a lamination. Information provided by Ex..