Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 201-67W171 Thermoplastic Vulcanizate  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 201-67W171 Thermoplastic Vulcanizate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion applications and has long term sealability, low temperature flexibility and heat weldability. This grade of Santoprene TPV is shear-dependent and is designed to be processed using specially adapted physical foam extrusion lines. It is polyolefin based and completely recyclable.Key Features:Can be foamed using water as the physical blowing agent or specific chemical blowing agents.Recommended for applications requiring excellent ozone resistance.EU and China RoHS compliant.Information provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 71

@Time 15.0 sec
71

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 6.90 MPa
1000 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 2.80 MPa

@Strain 100 %
406 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 450 %
450 %
Across Flow; ASTM D412 and ISO 37