Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 201-73W175 Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 201-73W175 Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.Recommended for applications requiring excellent flex fatigue resistance. Recommended for applications requiring excellent ozone resistance.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
.12 in; ASTM D2240
Tensile Strength at Break 8.48 MPa
1230 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 3.59 MPa
520 psi
Across Flow; ASTM D412
Elongation at Break 520 %
520 %
Across Flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Die Temperature 204 °C
400 °F
Extrusion
Melt Temperature 202 °C
395 °F
Extrusion
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour
Back Pressure 5.00 - 20.0 MPa
725 - 2900 psi
Extrusion
Descriptive Properties Value Comments
Color Natural Color
Form Pellets