Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 251-85W232 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 251-85W232 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retardants (non-furan emitting). It does not contain added antioxidants or metal deactivators. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Key Features: UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.Recommended for applications requiring excellent flex fatigue resistance.Recommended for applications requiring excellent ozone resistance.EU and China RoHS compliant.Applications: Automotive – Flame Retardant Connectors and SealsElectrical – Flame Retardant Connectors and seals; Flame Retardant Wire and Cable JacketUses: Automotive ApplicationsCable JacketingFlexible Cord JacketingWire & Cable Applications Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89

@Thickness 2.00 mm
89

@Thickness 0.0787 in
15 sec; ISO 868
Tensile Strength at Break 10.6 MPa
1540 psi
Across Flow; ASTM D412
Tensile Stress 4.50 MPa

@Strain 100 %
653 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 540 %
540 %
Across Flow; ASTM D412
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 35
Color Natural Color
Form Pellets
Users viewing this material also viewed the following: