Material Notes:
Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. SpectraSyn™ High Viscosity (PAO) products have high viscosity indices translate into improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn™ High Viscosity PAO basestocks are particularly suited for industrial oils requiring high stability under extreme operating conditions. SpectraSyn™ High Viscosity PAO products are frequently used in conjunction with lower viscosity fluids (PAO, mineral oils) as a viscosity booster to achieve a wide range of ISO VG industrial and automotive gear oils. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.850 g/cc

@Temperature 15.6 °C
0.0307 lb/in³

@Temperature 60.1 °F
ASTM D4052
Brookfield Viscosity 102000 cP

@Temperature -26.0 °C
102000 cP

@Temperature -14.8 °F
ASTM D2983
Viscosity Measurement 147
147
Index; ASTM D2270
Kinematic Viscosity 4840 cSt

@Temperature 0.000 °C
4840 cSt

@Temperature 32.0 °F
ASTM D445
40500 cSt

@Temperature -20.0 °C
40500 cSt

@Temperature -4.00 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 396 cSt
396 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 39 cSt
39 cSt
ASTM D445
Vapor Pressure 0.00120 bar

@Temperature 200 °C
0.900 torr

@Temperature 392 °F
ASTM D2879
Evaporation Loss 0.40 %

@Temperature 150 °C,
Time 79200 sec
0.40 %

@Temperature 302 °F,
Time 22.0 hour
ASTM D972
2.5 %

@Temperature 205 °C,
Time 23400 sec
2.5 %

@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Surface Tension 38.9 dynes/cm
38.9 dynes/cm
ASTM D1331A
Thermal Properties Metric English Comments
Pour Point -36.1 °C
-33.0 °F
ASTM D5950/D97
Flash Point 281 °C
538 °F
COC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.468
1.468
ASTM D1218
Electrical Properties Metric English Comments
Dielectric Constant 2.15
2.15
ASTM D924
Dielectric Breakdown 38900 V
38900 V
Chemical Properties Metric English Comments
Acid Value <= 0.10
<= 0.10
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point 319.3°F
ASTM D611
Color <0.5
ASTM D1500
Composition Water
<50 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000605 (g/cc)/°C
ASTM D1250
Fire point 604°F
COC, ASTM D92