Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -36.1 °C | -33.0 °F | |
ConocoPhillips Syncon® 680 Synthetic EP Gear Oil, AGMA No. 8EP Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is .. |
|||
Pour Point | -36.1 °C | -33.0 °F | ASTM D5950/D97 |
ExxonMobil SpectraSyn™ 40 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. Spect.. |
|||
Pour Point | -36.1 °C | -33.0 °F | |
ConocoPhillips Conoco® El Mar® Mid Ash Heavy Duty SAE 30 Conoco® El Mar Mid Ash Heavy Duty is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Pour Point | -36.1 °C | -33.0 °F | ASTM D5950/D97 |
ExxonMobil Synesstic™ 12 Synthetic Fluid Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit.. |
|||
Pour Point | -36.1 °C | -33.0 °F | |
ConocoPhillips HD Fleet™ 30 Engine Oil Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende.. |
|||
Pour Point | -36.1 °C | -33.0 °F | |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |