ExxonMobil Teresstic GT 32

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Teresstic GT 32.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teresstic GT is a high-quality turbine oil formulated to provide effective day-in and day-out performance of steam turbine and gas turbine electricity generators and mechanical drive systems. Teresstic GT is available in two ISO grades, 32 and 46.Teresstic GT is appropriate for a wide range of turbine applications, such as steam and gas turbines, compressors and pumps, including piston hydraulic pumps. It is an excellent multi-purpose lubricant. Additionally, Exxon offers Teresstic GT EP, specially formulated for anti-wear protection in heavily loaded gear turbine applications.
Physical Properties Metric English Comments
Specific Gravity 0.860 g/cc
0.860 g/cc
15°C; ASTM D1298
Viscosity Measurement 95
95
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 32 cSt
32 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.3 cSt
5.3 cSt
ASTM D445
Oxidative Stability 700 hour
700 hour
Rotating Bomb Oxidation Test (RBOT); ASTM D2272
Thermal Properties Metric English Comments
Pour Point -21.0 °C
-5.80 °F
ASTM D97
Flash Point 242 °C
468 °F
ASTM D92
Descriptive Properties Value Comments
Copper Strip Corrosion 1B
3 hrs @ 100°C
Demulsibility Time (min) 10
to 3 mL emulsion @ 54°C
Foam Sequence I, ASTM D981 0/0
Foam Sequence II, ASTM D893 0/0
Rust Prevention, Distilled Water pass
ASTM D665A
Rust Prevention, Synthetic Sea Water pass
ASTM D665B