Polymer Property : Oxidative Stability = 700 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Stability 700 hour
700 hour
Rotating Bomb Oxidation Test (RBOT); ASTM D2272
ExxonMobil Teresstic GT 32
Teresstic GT is a high-quality turbine oil formulated to provide effective day-in and day-out performance of steam turbine and gas turbine electricity generators and mechanical drive systems. Teress..
Oxidative Stability 700 hour
700 hour
Rotating Pressure Vessel Oxidation Test (RPVOT); ASTM D2272
ExxonMobil Teresstic M Series 32HT
The Teresstic M Series of products is the latest addition to the family of Teresstic turbine lubricant products, long recognized for their high quality and reliability. Teresstic M Series are design..
Oxidative Stability 700 hour
700 hour
Rotating Bomb Oxidation Test (RBOT); ASTM D2272
ExxonMobil Teresstic GT 32
Teresstic GT is a high-quality turbine oil formulated to provide effective day-in and day-out performance of steam turbine and gas turbine electricity generators and mechanical drive systems. Teress..
Oxidative Stability 700 hour
700 hour
Rotating Pressure Vessel Oxidation Test (RPVOT); ASTM D2272
ExxonMobil Teresstic M Series 32HT
The Teresstic M Series of products is the latest addition to the family of Teresstic turbine lubricant products, long recognized for their high quality and reliability. Teresstic M Series are design..
Oxidative Stability 700 hour
700 hour
ASTM D2272
ConocoPhillips Synterra™ 2 Hydraulic Oil, AGMA No. 2
Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids ..
Oxidative Stability 700 hour
700 hour
ASTM D2272
ConocoPhillips Synterra™ 3 Hydraulic Oil, AGMA No.3
Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids ..