Material Notes:
Mineral oil resistent
Physical Properties Metric English Comments
Density 1.40 - 1.44 g/cc
0.0506 - 0.0520 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 76
72 - 76
ISO R 868
Tensile Strength at Break >= 14.0 MPa
>= 2030 psi
ISO R 527
Elongation at Break >= 310 %
>= 310 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
Cold Flex; ISO 458/2
Descriptive Properties Value Comments
Thermal Stability (minutes) 90
CEI 20-34/3-2