Fainplast Compounds GS 69/F Flexible PVC, Injection Molding for Footwear

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GS 69/F Flexible PVC, Injection Molding for Footwear.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sandals
Physical Properties Metric English Comments
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 72
68 - 72
ISO R 868
Tensile Strength at Break 10.0 MPa
1450 psi
ISO R 527
Elongation at Break 300 %
300 %
ISO R 527
Abrasion 165
165
[mm³]; DIN 53516
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
Cold Flex; ISO 458/2