Fainplast Compounds GS 75/T Flexible PVC, Injection Molding for Footwear

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GS 75/T Flexible PVC, Injection Molding for Footwear.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crystal sandals
Physical Properties Metric English Comments
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77
73 - 77
ISO R 868
Tensile Strength at Break 14.0 MPa
2030 psi
ISO R 527
Elongation at Break 340 %
340 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
Cold Flex; ISO 458/2