Fainplast Compounds HAX HF 045 Halogen Free PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name HAX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HAX HF 045 Halogen Free PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose; improved fire performance
Physical Properties Metric English Comments
Density 1.50 - 1.54 g/cc
0.0542 - 0.0556 lb/in³
IEC 60811
Melt Index of Compound 8.5 g/10 min

@Load 21.6 kg,
Temperature 150 °C
8.5 g/10 min

@Load 47.6 lb,
Temperature 302 °F
Fainplast
Mechanical Properties Metric English Comments
Hardness, Shore D 46 - 52
46 - 52
IEC 60811
Tensile Strength at Break 12.5 MPa
1810 psi
IEC 60811
Elongation at Break 190 %
190 %
IEC 60811
Thermal Properties Metric English Comments
Oxygen Index 38 %
38 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+14 ohm-cm

@Temperature 20.0 °C
9.00e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257