Material Notes:
HAX HF 200 is a thermoplastic flame retardant compound, and halogen free on polyolefinic basis. It can be used for the production of energy, signal and control cables
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO R 1183
Melt Index of Compound 5.0 g/10 min

@Load 21.6 kg,
Temperature 150 °C
5.0 g/10 min

@Load 47.6 lb,
Temperature 302 °F
Fainplast
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
at 15"; ISO R 868
Tensile Strength at Break 12.0 MPa
1740 psi
ISO R 527
Elongation at Break 180 %
180 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 36 %
36 %
CEI 20-22
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Zone 1 130 - 150 °C
266 - 302 °F
Zone 2 130 - 160 °C
266 - 320 °F
Zone 3 140 - 160 °C
284 - 320 °F
Zone 4 140 - 160 °C
284 - 320 °F
Die Temperature 150 - 170 °C
302 - 338 °F
Head Temperature 150 - 165 °C
302 - 329 °F
Descriptive Properties Value Comments
Collar Temperature (°C) 165
Emission of Halogenidric acids (%) 0.1
Pressure Test at 80°C (%) 50
Water Absorption (mg/cm^2) 5