Fainplast Compounds PH 65/A Flexible PVC, Transparent Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Transparent
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PH 65/A Flexible PVC, Transparent Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Transparent profiles
Physical Properties Metric English Comments
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67
63 - 67
ISO R 868
Tensile Strength at Break 14.0 MPa
2030 psi
ISO R 527
Elongation at Break 360 %
360 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -34.0 °C
-29.2 °F
Cold Flex; ISO 458/2
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified