Fainplast Compounds PM 67/FR Flexible PVC, Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PM 67/FR Flexible PVC, Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Spiral pipes, UL 94 Class V0
Physical Properties Metric English Comments
Density 1.33 - 1.37 g/cc
0.0480 - 0.0495 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 69
65 - 69
ISO R 868
Tensile Strength at Break 12.0 MPa
1740 psi
ISO R 527
Elongation at Break 260 %
260 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -27.0 °C
-16.6 °F
Cold Flex; ISO 458/2
Flammability, UL94 V-0
V-0