Fainplast Compounds PMP 75/OP Flexible PVC, Extrusion Modified with PU

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PMP 75/OP Flexible PVC, Extrusion Modified with PU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High resistance to oil and hydrocarbon, with good abrasion resistance and elasticity
Physical Properties Metric English Comments
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77
73 - 77
ISO R 868
Tensile Strength at Break 16.0 MPa
2320 psi
ISO R 527
Elongation at Break 320 %
320 %
ISO R 527
Abrasion 90
90
[mm³]; DIN 53516
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
Cold Flex; ISO 458/2