Material Notes:
Rolling shutters
Physical Properties Metric English Comments
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ISO R 527
Tensile Strength, Yield 43.0 MPa
6240 psi
Elongation at Break 110 %
110 %
ISO R 527
Izod Impact, Unnotched 0.400 - 0.800 J/cm

@Temperature 23.0 °C
0.749 - 1.50 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 83.0 - 85.0 °C

@Load 5.00 kg
181 - 185 °F

@Load 11.0 lb
ISO R306