Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Quadrant EPP Cestlite™ ASTL Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
Vicat Softening Point | 82.8 - 108 °C | 181 - 226 °F | Average value: 97.7 °C Grade Count:72 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
Global ST-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 83.0 - 85.0 °C @Load 5.00 kg |
181 - 185 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 520/1 Rigid PVC, Extrusion Electric pipes |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ISO |
I. Stern N1921 General Purpose Crystal Polystyrene Features:Excellent ProcessabilityEasy FlowApplicationsDisposable PackagingHousewaresCosmetics PackagingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. In.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | VST/B/50; ISO 306 |
GEHR Plastics PE-ELS® Polyethylene HDPE A variant of PE-HD with improved electrical conductivity.Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties a.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ASTM D1525 |
Mitsui ADMER® NF548A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306B |
Lucite International Diakon® TD642 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Stir SpA HE 62 1 (PVC) Application: Extrusion rolling shutters - various profilesInformation provided by STIR SpA |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Stir SpA RI 1 A (PVC) Application: Spiral extrusion, shock resistantInformation provided by STIR SpA |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
Teknor Apex Sinvicomp SBB 3700 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
Teknor Apex Sinvicomp SBB 3704 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Good Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provide.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC) Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC) Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | ASTM D1525 |
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 83.0 - 85.0 °C @Load 5.00 kg |
181 - 185 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 220 Rigid PVC, Extrusion Rolling shutters |
|||
Vicat Softening Point | 83.0 °C | 181 °F | 1kg load; ASTM D1525 |
Eastman Eastar GN046 Copolyester, Natural Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Arkema Group OREVAC® 18370 Maleic Anhydride Modified Polyethylene OREVAC® 18370 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | ISO 306 |
Arkema Group OREVAC® 18380 Maleic Anhydride Modified Polyethylene OREVAC® 18380 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Vicat Softening Point | 82.8 °C | 181 °F | 50°C/hr; 50N; ASTM D1525 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
Vicat Softening Point | 83.0 °C | 181 °F | |
BASF Novolen® 2248 TC Polypropylene Nucleated grade with antistatic agent for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1005 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent film with high strength, shrinking at low temperature. Examples: curtain stretch, coextrusion, .. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1020 VB 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding rigid articles. Examples: closures, ice trays.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 83.0 °C | 181 °F | |
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |