Formosa Plastics Formolon® 45 PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 45 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Copolymer Dispersion Resin F-45 is a vinyl chloride vinyl acetate copolymer dispersion resin with low paste viscosities, excellent heat stability, and rapid fusion characteristics. F-45 has been successfully used in mechanically frothed foam, solid rug backing, laminating, fabric coating, flocking adhesives sealants, and many other applications.Note 1. 500 gm resin and 300 gm DOP, Hobart mixer mixed 5 min. @ No. 1 speed and 10 min. @ No. 2 speed, undeaerated.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Volatiles 0.40 %
0.40 %
ASTM D3030
Viscosity 1.1 cP
1.1 cP
Inherent; ASTM D1243
9000 cP
9000 cP
Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2
Relative Viscosity 2.5 cP
2.5 cP
QC-10-104
Brookfield Viscosity 9000 cP
9000 cP
20 rpm aged 2 hrs, See note 1; SPI-VD-T1
13500 cP
13500 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Vinyl Acetate Content 7.0 %
7.0 %
Bound; QC-10-105
Descriptive Properties Value Comments
Composition 0.02
Methanol Extract, ASTM D2222
Gelation Temperature 142°F
SPI-VD-T18
K-Value 72
Fikentscher's Constant
Users viewing this material also viewed the following: