Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fujipoly Industries FG-S Connector

Category Polymer , Thermoset , Silicone
Manufacturer Fujipoly Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fujipoly Industries FG-S Connector.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high current capacity make this series very versatile for many interconnect applications.Information provided by Fujipoly Industries
Physical Properties Metric English Comments
Specific Gravity 0.740 g/cc
0.740 g/cc
Silicone Sponge; JIS K6249/ASTM D792
1.02 g/cc
1.02 g/cc
Silicone Rubber; JIS K6249/ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 47
47
Silicone Rubber; JIS K6249/ASTM D2240
Tensile Strength, Yield 3.00 MPa
435 psi
Silicone Rubber; JIS K6249(Die #3)/ASTM D412
Elongation at Yield 240 %
240 %
Silicone Rubber; JIS K6249(Die #3)/ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+14 ohm-cm
7.00e+14 ohm-cm
Silicone Rubber; JIS-K-6249/ASTM D257
Surface Resistance 0.50 ohm
0.50 ohm
Contact Resistance, Electrode pad width = 0.25 mm
Insulation Resistance >= 2.00e+7 ohm
>= 2.00e+7 ohm
Gap = 0.25 mm
Descriptive Properties Value Comments
Color Clear or White
Silicone Rubber
Continuity Resistance <0.5 ohms
Current Carrying Capacity 30 mA/wire
Operating Compression Range H<3mm: 5-20%, 3mm