Polymer Property : Specific Gravity = 0.740 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.740 g/cc
0.740 g/cc
20/20°C
LyondellBasell ARCOPURE® High Purity MTBE, Methyl tertiary butyl ether
Information provided by Lyondell.
Specific Gravity 0.740 - 0.750 g/cc
0.740 - 0.750 g/cc
ASTM D891
LG Chemical c-Pentane
Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o..
Specific Gravity 0.740 g/cc
0.740 g/cc
Silicone Sponge; JIS K6249/ASTM D792
Fujipoly Industries FG-S Connector
Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre..
Specific Gravity 0.740 g/cc
0.740 g/cc
Silicone Sponge; JIS K6249/ASTM D792
Fujipoly Industries FG-S Fine Connector
Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre..
Specific Gravity 0.740 g/cc
0.740 g/cc
ASTM D792
Spartech Polylite Foamed Polyolefin Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Specific Gravity 0.740 g/cc
0.740 g/cc
Shin-Etsu Silicones X-33-514 Silicone Primer
Information Provided by Shin-Etsu Silicones of America, Inc.
Specific Gravity 0.740 g/cc
0.740 g/cc
BCC Products MB 2001 Urethane Foam Modeling Board
MB2001 is a general purpose light weight urethane board engineered specifically to meet the tooling requirements of a wide range of applications for the automotive/aerospace, prototype, foundry, and..